| Grade : | S235JR |
| Number: | 1.0038 |
| Standard: | EN 10025 - 2 : 2004 Technical delivery conditions for non-alloy structural steels |
| Classification: | Non-alloy structural steels |
| Applications: | Non-alloy steel for structural purposes |
|
Nominal thickness =< 40(mm) C max = 0.17
|
| C | Mn | P | S | N | Cu | CEV |
| max 20 | max 1.4 | max 0.04 | max 0.04 | max 0.012 | max 0.55 |
max 0.38 |
Mechanical properties of grade ASTM A29
| Temperature | -20 | 0 | 20 |
| Notch impact test. Min. absorbed energy | 27 | 27 | 27 |
| Nominal thickness (mm) | to 16 | 16 - 40 | 40 - 63 | 63 - 80 | 80 - 100 | 100 - 125 |
| ReH - Minimum yield strength (MPa) | 235 | 225 | 215 | 215 | 215 | 195 |
| Nominal thickness (mm) | 3 - 100 | 100 - 125 |
| Rm -Tensile strength (MPa) | 360-510 | 350-500 |
| Nominal thickness (mm) | 3 - 40 | 40 - 63 | 63 - 100 | 100 - 125 |
| A - Minimum elongation Lo = 5,65 √ So (%) | 26 | 25 | 24 | 22 |
| Weldability: This steel grade is generally suitable to welding |
| SA - |
Germany DIN,WNr |
Japan JIS |
France AFNOR |
England BS |
Canada HG |
European old EN |
Belgium NBN |
Spain UNE |
China GB |
Sweden SS |
Austria ONORM |
Norway NS |
Russia GOST |
International ISO |
Portugal NP |
India IS |
||||||||||||||||||||||||||
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|