Location » Home » Grades > Special Alloy > EN NiCr22Mo9Nb

Tags

Chemical composition % of the ladle analysis of grade EN NiCr22Mo9Nb

0.03-0.10 Max 0.50 0.50 0.020 0.015 20.0-23.0 Min58.0 8.00-10.0 3.15-4.15 Max 0.40
Euronorm Stainless Steel, EN NiCr22Mo9Nb
Mechanical properties of grade EN NiCr22Mo9Nb
Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
625 (≥) 967 (≥) 22 14 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Physical properties of grade EN NiCr22Mo9Nb
Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
159 (≥) 948 (≥) 31 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 413
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
442 666 899
EN NiCr22Mo9Nb Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED
Cross Reference Table(Equivalent Grade)
Grade Standard Country Application
NiCr22Mo9Nb
Heat resisting steels and nickel alloys
2.4856
Heat resisting steels and nickel alloys
NiCr22Mo9Nb
Nickel and nickel alloy forgings

Enquiry