Chemical composition % of the ladle analysis of grade ISO X6NiCrSi36 19

Max 0.08 0.75-1.5 Max 2.0 Max 0.030 Max 0.030 17.0-20.0 34.0-37.0 Max 1.0 Max 0.005 Sn: Max 0.025
ISO standard  Austenite size heat resistant steel
Mechanical properties of grade ISO X6NiCrSi36 19
Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
525 (≥) 866 (≥) 24 24 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Physical properties of grade ISO X6NiCrSi36 19
Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
347 (≥) 272 (≥) 42 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
915 847 674
ISO X6NiCrSi36 19 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED
Cross Reference Table(Equivalent Grade)
Grade Standard Country Application
X6NiCrSi36-19
Heat-resistant steels